How to use plastic wood edge banding correctly

Views : 557
Update time : 2017-11-14 14:48:58
 
How to use plastic wood edge banding correctly?
Edge banding: Edge banding is the section of the plate solid seal, to avoid the surrounding environment and the use of the process.

Specifications: Thickness of the general 0.3mm-3mm,broadband 12mm-100mm, can also be customized according to requirements.


Judge good or bad: the surface texture and color consistent with the plate, the surface is smooth, non-convex, the same width, uniform thickness, trimming not white, trimming color  and face close.

Hot melt adhesive: also known as edge banding adhesive, the main ingredient is resin, is a solid adhesive, reaches a certain melting point can become a liquid, can be used for bonding sheet and edge banding. It's non-toxic and tasteless, are environmentally friendly chemical products. Color transparent, of different colors.

Related News
Read More >>
What are the characteristics of environmentally friendly edge sealing hot melt adhesives? What are the characteristics of environmentally friendly edge sealing hot melt adhesives?
Oct .20.2022
The solid content is 100%, and it has void filling properties, which avoids the defects such as deformation, dislocation and shrinkage of the adhered parts caused by edge curling, air bubbles and cracking.
Appearance And Prospect Of Edge Sealing Hot Melt Adhesive Appearance And Prospect Of Edge Sealing Hot Melt Adhesive
Sep .22.2022
Environmentally friendly edge sealing hot melt adhesive is a green and pollution-free environmental friendly adhesive.
What kinds of situations often occur when hot melt adhesive particles are used in furniture edge sealing? What kinds of situations often occur when hot melt adhesive particles are used in furniture edge sealing?
Aug .26.2022
1. Black edge phenomenon: The hot melt machine has not been cleaned for a long time, and the glue itself has carbonization phenomenon.
Reasons for the open edge of the edge band Reasons for the open edge of the edge band
Aug .13.2022
The moisture content of the edge banding wood is unqualified (>18%), and the natural drying during the use of the door leaf produces internal stress, resulting in cracking and deformation of the edge banding.