(一) What type of temperature is hot melt adhesive? how to use it? Professionals tell you

Views : 669
Update time : 2018-10-11 17:10:11
Low temperature hot melt adhesive

      Product properties: EVA edge-sealing hot melt adhesive, appearance of white particles, non-toxic and environmentally friendly.
 
      Product features: Wide application range, long opening time; suitable for manual / semi-automatic edge banding machine; good fluidity, less glue consumption;
 
      Technical parameters:
Viscosity value 25,000mpa.s (Brinell) at 150 °C
  
Density 1.35g/cm    
Softening point 80°C (ring and ball method) Anti-hot spot 58°C
Operating parameters: Material temperature>15 °C
Ambient temperature>15°C
Material moisture content 8%--10%
Glue temperature 120--130°C
Rubber roll temperature 130--150 °C
pressure 3--5kg/cm2 feed rate >4 m/min

 
      Scope of application: Suitable for PVC, ABS, decorative paper and other edge-sealing materials, especially 0.4mm thick and low temperature resistant PVC edge banding; manual/semi-automatic curved edge banding machine for 4--6m/min feed speed;
 

Related News
Read More >>
What are the characteristics of environmentally friendly edge sealing hot melt adhesives? What are the characteristics of environmentally friendly edge sealing hot melt adhesives?
Oct .20.2022
The solid content is 100%, and it has void filling properties, which avoids the defects such as deformation, dislocation and shrinkage of the adhered parts caused by edge curling, air bubbles and cracking.
Appearance And Prospect Of Edge Sealing Hot Melt Adhesive Appearance And Prospect Of Edge Sealing Hot Melt Adhesive
Sep .22.2022
Environmentally friendly edge sealing hot melt adhesive is a green and pollution-free environmental friendly adhesive.
What kinds of situations often occur when hot melt adhesive particles are used in furniture edge sealing? What kinds of situations often occur when hot melt adhesive particles are used in furniture edge sealing?
Aug .26.2022
1. Black edge phenomenon: The hot melt machine has not been cleaned for a long time, and the glue itself has carbonization phenomenon.
Reasons for the open edge of the edge band Reasons for the open edge of the edge band
Aug .13.2022
The moisture content of the edge banding wood is unqualified (>18%), and the natural drying during the use of the door leaf produces internal stress, resulting in cracking and deformation of the edge banding.